Glass UV hot stamping paste solves the problem of adhesion on the glass surface, and can be connected to hot stamping paper, which can produce metal color on the glass and surface. It makes the hot-stamped substrates appear more exquisite, textured and noble, so that the users who use the products feel the manufacturer's cherishment and care for the users.
The glass UV hot stamping paste after being baked at a low temperature, the hot stamping operation can be carried out with high efficiency and smooth hot stamping effect. After drying, the hot stamping paste has good hardness and stable molecular structure, which effectively reduces the cracking, wrinkling, popping, air bubbles and other phenomena of hot stamping. Glass UV hot stamping paste has high transparency and strong adhesion to the hot stamping surface, and has no repulsion such as wrinkling with the hot stamping surface. It is resistant to alcohol wiping and has excellent adhesion after baking.
The hot stamping paste is flexible, stretchable and has strong adhesion. It has good adhesion on the surface of spray glazed bottles, matte bottles and white glass bottles. Suitable for both flat hot stamping and embossing hot stamping, high efficiency.
The quality of hot stamping is affected by many factors, especially since hot stamping is performed after silk screen printing, the printing effect, the thickness of UV hot stamping paste, and the properties of UV hot stamping paste will directly affect the effect of hot stamping. Therefore, the following issues should be noted:
1) Hot stamping should be done after the hot stamping paste is dry. If the hot stamping is started when the hot stamping paste layer is not dry, it is easy to cause the failure of pulling off the ink layer since the ink is not adhered firmly, so that the hot stamping cannot be applied.
2) If hot stamping on the base color, the base color hot stamping paste layer should not be too thick , try to make a deep paste and thin printing to avoid overprinting, in order to avoid the hot stamping paste being too thick and not firmly attached, causing hot stamping Poor printing, sticky, or even pull off the paste layer and other undesirable phenomena.In addition, when hot stamping the solid background color, the hot stamping temperature should be appropriately reduced, so that the hot stamping effect is more ideal.